Causes and solutions of top whiteness in injection molding products

Release time:2021-08-16

When the plastic parts of injection products are ejected from the mold, if the ejector pin is used, the ejector rod will often leave deep or shallow marks on the plastic parts. If these traces are too deep, the so-called top white phenomenon will appear. In serious cases, the so-called top explosion will occur when the plastic parts are pushed through.


The main reason for the whiteness of plastic parts is that the product has a large mold adhesion force, and the ejection part on the plastic parts causes white marks at the ejection part of the ejector rod. The specific reasons and improvement methods are as follows:


1. Back mold temperature is too low or too high: adjust the appropriate mold temperature.


2. Too fast ejection speed: slow down the ejection speed.


3. With demoulding chamfer: overhaul the mold (polishing).


4. The ejection of finished products is unbalanced (the ejection leaf spring is broken): repair the mold (make the ejection balanced).


5. Insufficient number of thimbles or improper position: increase the number of thimbles or change the position of thimbles.


6. Vacuum occurs in the mold during demoulding: clean the dirt in the ejector pin hole to improve the air inlet effect.


7. The finished bone and column positions are rough (inverted): polish each bone and column position.


8. High injection pressure or holding pressure: reduce the pressure appropriately.


9. The demoulding angle of the finished mold is too small: increase the demoulding angle of the rear mold.


10. Improper action time or position of side slider: repair the mold (make the core pulling action normal).


11. Ejection area is too small or ejection speed is too fast: increase the ejection area or slow down the ejection speed.


12. The injection speed of the last section is too fast (Burr): slow down the injection speed of the next section.


These are the reasons and solutions for the whitening of injection molded products.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
伊人久久大香线蕉综合75| 日韩人妻无码一区二区三区免费| 亚洲精品日韩一区二区电影| 国产一区二区三区在线观看| 精品久久久久久久免费人妻| 性无码专区无码| 国产50部艳色禁片无码| 久久99国产综合精品尤物| 精品乱子伦一区二区三区| 任你躁x7x7x7x7在线观看| 亚洲熟妇色xxxxx欧美老妇| 久久久久久无码AV成人影院| 国产性猛交╳xxx乱大交| 国产伦精品一区二区三区视频| 亚洲av综合色区无码一区爱av| 色综合久久中文字幕无码| 人妻巨大乳挤奶水HD免费看| 奶头被民工吸的又大又黑| 精品国品一二三产品区别在线观看| 99精品久久久久久久婷婷| 五月天中文字幕mv在线| 色综合色综合色综合色欲 | 99热久久精里都是精品6| 国产老熟女精品一区| 国产性生交xxxxx免费| 国产老色鬼无码免费视频| 99re6在线视频精品免费| 无码人妻| 曰本丰满熟妇XXXX性| 精品欧美一区二区在线观看| 国产96在线 | 欧美| 狠狠色成人一区二区三区| 无码人妻丰满熟妇精品区| 亚洲国产精品一区二区美利坚| 国产a√精品区二区三区四区| 精品久久久久久久无码| 国产八十老太另类| 亚洲av中文无码乱人伦在线视色| 婷婷丁香五月久久综合啪啪图区| 中文无码亚洲精品制服丝袜| 小雪第一次尝到又大又粗|